MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Aperam Resistohm® 20 Resistant Alloys-Nickel Chromium Alloys
Categories: Metal; Ferrous Metal

Material Notes: Resistohm 20 is placed at the limit between heat resistant alloys and stainless steels. It can be used for heating elements at low temperature, or as cold connections of a furnace.

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 220
Tensile Strength 750 MPa
Tensile Strength, Yield 400 MPa
Elongation at Break >= 30 %on 100 mm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000095 ohm-cmTemperature coefficient = 0.00033/°C from 20 - 100°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.5 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 11.5 W/m-K
@Temperature 120 °C
Melting Point 1390 °C
Maximum Service Temperature, Air 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 25 %
Iron, Fe 55 %
Nickel, Ni 20 %
 
Descriptive Properties
Creeping point20at 800°C
 4at 1000°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aperam Resistohm® 80 Resistant Alloys-Nickel Chromium Alloys
H.C. Starck Amperit® 586.1 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
Alloy Wire International RW 80 Ni-Cr Resistance Wire
H.C. Starck Amperit® 582.072 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
H.C. Starck Amperit® 586.054 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)

NPERA085 / 194874

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.