MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Perkadox AIBN Pharmaceuticals glo 2,2'-Azodi(isobutyronitrile)
Categories: Other Engineering Material

Material Notes: 2,2’-Azodi(isobutyronitrile) (Perkadox AIBN) is the (azo)initiator most commonly employed in radical reactions, especially those using tri-n-butyltin hydride. At temperatures above about 60°C, Perkadox AIBN decomposes with evolution of nitrogen to generate isobutyronitrile radicals. Major examples of reactions are cyclizations and halogenation.

CAS number: 78-67-1

EINECS/ELINCS No.: 201-132-3

Applications: Perkadox AIBN can be successfully used for bulk, solution, suspension polymerization of a wide variety of monomers, such as styrene, vinyl chloride, vinylidene, acrylonitrile, acrylates and methacrylates. Perkadox AIBN does not form oxygenated residues and does not cause oxidative degradation of pigmented of dyed polymer systems. For this reason, the color stability or transparent, dyed polymers, such as polymethylmethacrylate, is improved. 2,2’- Azodi(isobutyronitrile) (Perkadox AIBN) is also the (azo)initiator most commonly employed in radical reactions, especially those using tri-n-butyltin hydride.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.600 g/cc0.0181 - 0.0217 lb/in³
Density 1.11 g/cc0.0401 lb/in³
Half-life  0.100
@Temperature 101 °C
0.100
@Temperature 214 °F
[hr]
 1.00
@Temperature 82.0 °C
1.00
@Temperature 180 °F
[hr]
 10.0
@Temperature 64.0 °C
10.0
@Temperature 147 °F
[hr]
Molecular Weight 164.2 g/mol164.2 g/mol
Storage Temperature <= 25.0 °C<= 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 104 °C219 °F
Decomposition Temperature 50.0 °C122 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY778 / 286301

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.