MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Aluminum Bronze, UNS C95410, Copper Casting Alloy, TQ50 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: Good wear resistance, heat treatable. Except where noted, all property values are for sand casting.

Recommended Casting Methods: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand.

Applications:Pump impellers, bearings, gears, worms, bushings, valve seats and guides, rolling mill slippers, slides, nonsparking hardware.

Classified under: Aluminum bronzes. ASTM B148; formerly ASTM B148-9C

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.45 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 1953000 kg
Hardness, Rockwell B 94
Tensile Strength, Ultimate 620 MPa
Tensile Strength, Yield 310 MPa
Elongation at Break 8.0 %in 50 mm
Reduction of Area 6.0 %
Modulus of Elasticity 110 GPa
Compressive Strength 1070 MPa
Poissons Ratio 0.316
Fatigue Strength 240 MPa
@# of Cycles 1.00e+8
Reverse Bending
Machinability 60 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 41.0 GPa
Izod Impact 15.0 J
Charpy Impact 9.00 JKeyhole
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000133 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.216 kA/m field strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 59.0 W/m-K
@Temperature 20.0 °C
Melting Point 1025 - 1040 °C
Solidus 1025 °C
Liquidus 1040 °C
Shrinkage 1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 620 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 10 - 11.5 %
Copper, Cu >= 83 %
Iron, Fe 3.0 - 5.0 %
Manganese, Mn <= 0.50 %
Nickel, Ni 1.5 - 2.5 %Includes Co

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276
ATI Allegheny Ludlum Grade 3 Titanium (UNS R50550)
ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal
Copper, UNS C62300 (Aluminum Bronze 9%), Annealed Rod
Eagle Brass 519 Phosphor Bronze 6%, Extra Hard

MC95410b2 / 171654

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.