Electrically conductive urethane adhesive, silver-filled, flexible low modulus, low outgassing APTEK 2210-A/B is a two component, silver-filled, urethane adhesive designed for application where flexibility and electrically conductivity are required. APTEK 2210-A/B is a 100% solid adhesive displaying excellent adhesion to plastic metal substrates.Non-TDI based for safety; Very flexible/low modulus to absorb stress buildup during thermal cycling; Excellent adhesion to ceramic and various substrates; Low Tg(<-60ºC) for excellent low temperature performance APTEK 2210A is a silver filled polyol resin. APTEK 2210B is an organic isocyanate. Information provided by Aptek Laboratories, Inc. |