MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borlink™ LE0516 Polyethylene Compound, Crosslinkable, Semiconductive
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LE0516 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0516 is intended for strippable outer semi conductive shielding of XLPE medium voltage cables with rated voltages up to 36 kV. Specifications: AEIC CS8-00 (1st edition); BS 6622; ICEA S-94-649; IEC 60502; NF C33-223; NF C33-226; and UTE C 33-223.

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183/ISO 1872-2
Water Absorption 0.080 %0.080 %Karl Fischer-titration
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 15.0 MPa2180 psiISO 527
Elongation at Break 400 %400 %25mm/min; ISO 527
Tensile Set 0.00 %
@Temperature 200 °C
0.00 %
@Temperature 392 °F
Permanent Deformation at 0.2 MPa after 25% elongation under load; IEC 60811-2-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  <= 100 ohm-cm
@Temperature 23.0 °C
<= 100 ohm-cm
@Temperature 73.4 °F
ISO 3915
 <= 1000 ohm-cm
@Temperature 90.0 °C
<= 1000 ohm-cm
@Temperature 194 °F
ISO 3915
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 °C536 °Fmaximum surface temperature, curing tube
Feed Temperature >= 40.0 °C>= 104 °F
Melt Temperature 120 - 140 °C248 - 284 °F
Drying Temperature 40.0 °C104 °Fdrying temperature; under agitation with a dewpoint of -35°C
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Göttfert Elastograph (Nm)0.6-1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis FL5580 High Density Polyethylene
Borealis Borlink™ LE0594 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Borealis Borlink™ LE0310-99 Polyethylene Thermoplastic Semiconductive Compound
Borealis Borlink™ LE0520 Polyethylene Compound, Crosslinkable, Semiconductive
Borealis Borlink™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables

PBOREA508 / 108767

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.