MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Molded

Material Notes: Description

Formion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductility.
Application

Formion® FI 105E is targeted for exterior or interior appearance or packaging applications in film, blow molding, thermoforming or extrusion applications, which may require high or low gloss, excellent colorability or transparency.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccISO 1183/1
Linear Mold Shrinkage 0.0060 - 0.018 cm/cm
@Thickness 3.20 mm
72 hr; ISO 294
Melt Index of Compound 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 6015 sec delay; ISO 868
Tensile Strength, Ultimate 21.0 MPaat max load; ISO 527
Tensile Strength, Yield 21.0 MPaISO 527
Elongation at Break 275 %ISO 527
Flexural Modulus 0.360 GPaTangent; ISO 178
Izod Impact, Notched (ISO) NBISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C
@Thickness 3.20 mm
ISO 75
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer
Overview of materials for Ionomer, Molded
Overview of materials for Ionomer, Film Grade
A. Schulman FORMION™ FI 301 Ionomer

PASHU019 / 24983

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.