EUDRAGIT NE 40 D is the aqueous dispersion of a neutral copolymer based on ethyl acrylate and methyl methacrylate. Physical properties: It is a milky-white liquid of low viscosity with a faint characteristic odour. Characteristics: - No plasticizer required
- Highly flexible
- Suitable for matrix structure
CAS number: 9010 – 88 – 2Chemical/ IUPAC name: Poly(ethyl acrylate-co-methyl methacrylate) 2:1 INCI name: Acrylates Copolymer Information provided by Evonik |