MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Pluracol® 1538 Slabstock Foam Polyol
Categories: Fluid

Material Notes: Description: Pluracol® 1538 polyol is intended for the production of Visco-Elastic foam typically formulated with another base product such as Pluracol 593 polyol. The combination of these two immiscible polyols provide a unique technology foundation in the manufacture of ViscoElastic foams intended for bedding, pillow, and seating applications. Pluracol 1538 polyol is a nominal 3000 MW product with a light EO cap. This product contains a LVI inhibitor package.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.989 g/cc
@Temperature 54.5 °C
 1.00 g/cc
@Temperature 37.8 °C
 1.01 g/cc
@Temperature 21.1 °C
Viscosity 250 cP
@Temperature 54.5 °C
 300 cP
@Temperature 37.8 °C
 700 cP
@Temperature 21.1 °C
Molecular Weight 3000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.010STI 3063/3161
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.16 J/g-°C
Thermal Conductivity 0.125 W/m-K
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %STI 3062
 
Descriptive Properties
ColorClear Liquid
Hydroxyl Number56.0 mg KOH/gSTI 3007/3162

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Pluracol® 1528 FF Molded Foam Polyol
BASF Pluracol® 1168 Rigid Polyol
AGC PREMINOL® S 4013F Polyol
Dow VORANOL™ 4701 Polyether Polyol
Dow VORANATE™ T-80 toluene diisocyanate (TDI)

PBASG0777 / 132410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.