MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® B27 E 01 PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Ultramid B27 E 01 is a low viscosity general-purpose, extrusion PA6 grade well suited for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or legislations for other countries will be provided on request.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Water Absorption 9.5 %ISO 62
Moisture Absorption at Equilibrium 2.6 %23°C/50% R.H.; ISO 62
Relative Viscosity 2.7 cPISO Test; 96 % SAV
Viscosity Number 150 cm³/g
Linear Mold Shrinkage 0.010 cm/cmASTM Data; MD
Melt Flow 130 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 80.0 MPa2 in/min; ASTM Test
 90.0 MPa50mm/min; ISO 527
Elongation at Break 15 %50mm/min, Nominal strain; ISO 527
Elongation at Yield 4.5 %50mm/min; ISO 527
Tensile Modulus 3000 MPa1mm/min; ISO 527
 3000 MPaASTM Test
Izod Impact, Notched 0.480 J/cm
@Temperature -40.0 °C
ASTM Test
 0.530 J/cm
@Thickness 3.17 mm
ASTM Test
Charpy Impact Unnotched NBISO 179
 NB
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 0.800 J/cm²ISO 179
 NB
@Temperature -30.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.010
@Frequency 100 Hz
IEC 60250
 0.023
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM Test
CTE, linear, Parallel to Flow 85.0 µm/m-°CISO 11359
Melting Point 220 °C10 K/min
 220 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 160 °CASTM Test
 160 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °CASTM Test
 65.0 °CISO 75
Vicat Softening Point 204 °C(50 °C/h / 50N) - B/50; ISO 306
Glass Transition Temp, Tg 60.0 °C10 K/min; ISO 11357-1/-3
Oxygen Index 26 %ISO 4589-1/-2
 
Compliance PropertiesOriginal ValueComments
FDA Yes21 CFR 177.1500
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingOther Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B27 E 01 PA6 (Conditioned)
BASF Ultramid® B27 E PA6
BASF Ultramid® B32 01 PA6 (Dry)
BASF Ultramid® B3K PA6 (Dry)
BASF Ultramid® B27 03 PA6

PBASF9283 / 85047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.