MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-PFM16 High Effective Impact Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GY- PFM16 is a high effective impact modifier which can be widely used to PP, engineering plastic and general plastic. GY- PFM16 can enhance both chemical and physical properties, including weather-resistant, impact-resistant, strong elongation strength, excellent durability of low temperature and good optical capacity. The applications are package, film, compound, blow molding, foam products…etc. GY- PFM16 not only increases impact-resistant of plastic product, but also brings added value and competitive power for customers.

Advantages:

  • Improve flexible ability and impact toughness for plastic
  • Good chemical resistance
  • Good foam ability due to LCB (long chain branching) properites
  • High melt strength properties between general PP an HMSPP
  • Enhance scratch resistance
  • Increase weather resistance for plastic and elastomer
  • Suitable for transparent or colorful products.
  • lower shrinkage and compression set
  • Improve color ability, surface finish, and soft touch
  • High flow ability
  • Good bonding ability with PP and mPE
  • Match with filler (talc, oil, calcium carbonate..etc)
  • Good workability and compatibility
Applications:
  • Polypropylene (PP)
  • PE : HDPE,LDPE,LLDE
  • EVA
  • TPR,TPE, TPE modified
  • Film blowing
  • blow molding and foam products
  • Hollow extrusion and calendering
  • Various film
  • Fiber
  • Sheet
  • Polyolefin modified
  • Plug-in for internal and external
  • Non-woven fabric
  • Package
  • Personal care supplies
  • Wire & cable
  • Soft-touch handle
  • Foam products for leisure, sport and general consumer.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 1.4 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 1.94 MPa
@Strain 100 %
 2.24 MPa
@Strain 300 %
Elongation at Break >= 2000 %
Flexural Strength >= 6.89 MPa
Flexural Modulus 12.3 MPa1% secant
Tear Strength 34.3 kN/mC mold
Tensile Set 18 %
 
Descriptive Properties
Appearancepellet
Colortransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN285 / 266593

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.