MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior drawdown and enhanced toughness. Enable 20-05 resins are available for blown film, both formulated and non-formulated. A heavily stabilized formulation for cast film processing is also available.

Availability: Latin America, North America and South America

Additive:

    Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Agricultural Film
  • Blown Film
  • Cast Film
  • Cast Stretch Film
  • Collation Shrink
  • Food packaging
  • Form Fill and Seal Packaging
  • Heavy Duty Bags
  • Lamination Film
  • Multilayer Packaging Film
  • Shrink Film
  • Stand Up Pouches
  • Stretch Film

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccExxonMobil method
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1500 psiASTM D882
Film Tensile Strength at Yield, TD 1600 psiASTM D882
Film Elongation at Break, MD 480 %ASTM D882
Film Elongation at Break, TD 470 %ASTM D882
Puncture Energy 32.0 in-lbExxonMobil Method
Elmendorf Tear Strength MD 90 gASTM D1922
Elmendorf Tear Strength TD 580 gASTM D1922
Dart Drop Test 210 gASTM D1709A
Film Tensile Strength at Break, MD 8700 psiASTM D882
Film Tensile Strength at Break, TD 8100 psiASTM D882
1% Secant Modulus, MD 31000 psiASTM D882
1% Secant Modulus, TD 35000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 237 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesOriginal ValueComments
Haze 8.0 %ASTM D1003
Gloss 56 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force12 lbfExxonMobil Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin
ExxonMobil Enable™ 20-10HA Metallocene Polyethylene Resin
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin

PEX99002 / 175239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.