MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Overview of materials for Polypropylene, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.800 - 1.90 g/ccAverage value: 1.10 g/cc Grade Count:371
Filler Content 10.0 - 50.0 %Average value: 24.3 % Grade Count:34
Water Absorption 0.0100 - 0.100 %Average value: 0.0319 % Grade Count:97
Moisture Absorption at Equilibrium 0.0100 - 0.200 %Average value: 0.0417 % Grade Count:6
Water Absorption at Saturation 0.100 - 0.150 %Average value: 0.133 % Grade Count:3
Maximum Moisture Content 0.0100 - 0.0200Average value: 0.0125 Grade Count:4
 0.150 - 0.200
@Temperature 120 - 120 °C
Average value: 0.175 Grade Count:2
 0.150 - 0.200
@Time 299 - 299 sec
Average value: 0.175 Grade Count:2
Linear Mold Shrinkage 0.000100 - 0.0500 cm/cmAverage value: 0.0132 cm/cm Grade Count:269
Linear Mold Shrinkage, Transverse 0.00400 - 0.0243 cm/cmAverage value: 0.0138 cm/cm Grade Count:60
Melt Flow 0.300 - 140 g/10 minAverage value: 11.5 g/10 min Grade Count:283
Ash 15.0 - 25.0 %Average value: 20.0 % Grade Count:4
 40.0 - 44.0 %
@Temperature 625 - 625 °C
Average value: 42.0 % Grade Count:1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100Average value: 100 Grade Count:4
Hardness, Rockwell R 69.0 - 105Average value: 90.9 Grade Count:25
Hardness, Shore A 66.0 - 69.0Average value: 67.8 Grade Count:6
Hardness, Shore D 60.0 - 80.0Average value: 70.7 Grade Count:32
Tensile Strength, Ultimate 7.50 - 300 MPaAverage value: 32.2 MPa Grade Count:241
 7.00 - 45.0 MPa
@Temperature 60.0 - 90.0 °C
Average value: 16.9 MPa Grade Count:4
Tensile Strength, Yield 2.07 - 96.0 MPaAverage value: 30.0 MPa Grade Count:151
Elongation at Break 1.00 - 700 %Average value: 58.1 % Grade Count:284
 4.00 - 20.0 %
@Temperature 60.0 - 90.0 °C
Average value: 66.2 % Grade Count:8
Elongation at Yield 2.00 - 350 %Average value: 29.4 % Grade Count:52
 2.50 - 10.0 %
@Temperature 60.0 - 90.0 °C
Average value: 7.56 % Grade Count:8
Modulus of Elasticity 0.800 - 11.8 GPaAverage value: 2.35 GPa Grade Count:154
 0.300 - 5.70 GPa
@Temperature 60.0 - 90.0 °C
Average value: 1.26 GPa Grade Count:8
Flexural Yield Strength 17.9 - 300 MPaAverage value: 43.4 MPa Grade Count:187
Flexural Modulus 0.621 - 8.00 GPaAverage value: 2.03 GPa Grade Count:313
Izod Impact, Notched 0.107 J/cm - NBAverage value: 0.865 J/cm Grade Count:247
 0.100 - 0.750 J/cm
@Temperature -20.0 - 0.000 °C
Average value: 0.317 J/cm Grade Count:29
Izod Impact, Unnotched 0.300 - 5340 J/cmAverage value: 5.92 J/cm Grade Count:68
 0.150 - 0.400 J/cm
@Temperature 0.000 - 0.000 °C
Average value: 0.254 J/cm Grade Count:8
Izod Impact, Notched (ISO) 2.00 - 60.0 kJ/m²Average value: 7.17 kJ/m² Grade Count:55
 2.00 - 10.0 kJ/m²
@Temperature -30.0 - -20.0 °C
Average value: 3.95 kJ/m² Grade Count:10
Izod Impact, Unnotched (ISO) 44.0 - 98.0 kJ/m²Average value: 70.3 kJ/m² Grade Count:6
 13.0 - 13.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 13.0 kJ/m² Grade Count:2
Charpy Impact Unnotched 1.00 J/cm² - NBAverage value: 4.29 J/cm² Grade Count:61
 0.650 - 999.9 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 3.16 J/cm² Grade Count:26
Charpy Impact, Notched 0.150 - 9.00 J/cm²Average value: 0.626 J/cm² Grade Count:72
 0.0400 - 1.40 J/cm²
@Temperature -30.0 - -20.0 °C
Average value: 0.266 J/cm² Grade Count:30
Gardner Impact 0.904 - 260 JAverage value: 26.8 J Grade Count:24
Dart Drop, Total Energy 2.71 - 14.9 JAverage value: 8.59 J Grade Count:3
Dart Drop Total Energy 1.44 - 8.54 J/cmAverage value: 6.10 J/cm Grade Count:4
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 10.0 - 1.00e+17 ohm-cmAverage value: 4.43e+15 ohm-cm Grade Count:83
Surface Resistance 1000 - 1.00e+16 ohmAverage value: 2.17e+15 ohm Grade Count:48
Static Decay 0.500 - 2.00 secAverage value: 1.10 sec Grade Count:5
Dielectric Constant 2.10 - 3.06Average value: 2.53 Grade Count:13
Dielectric Strength 17.7 - 43.0 kV/mmAverage value: 28.8 kV/mm Grade Count:50
Dissipation Factor 0.00120 - 0.0100Average value: 0.00360 Grade Count:6
Arc Resistance 60.0 - 180 secAverage value: 124 sec Grade Count:6
Comparative Tracking Index 250 - 600 VAverage value: 570 V Grade Count:97
Hot Wire Ignition, HWI 7.00 - 60.0 secAverage value: 26.8 sec Grade Count:4
High Amp Arc Ignition, HAI 120 arcsAverage value: 120 arcs Grade Count:4
High Voltage Arc-Tracking Rate, HVTR 0.000 - 330 mm/minAverage value: 116 mm/min Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 37.8 - 90.0 µm/m-°CAverage value: 61.1 µm/m-°C Grade Count:12
Thermal Conductivity 0.170 - 0.303 W/m-KAverage value: 0.258 W/m-K Grade Count:3
Melting Point 130 - 170 °CAverage value: 162 °C Grade Count:56
Maximum Service Temperature, Air 60.0 - 130 °CAverage value: 89.6 °C Grade Count:24
Hot Ball Pressure Test 75.0 - 145 °CAverage value: 122 °C Grade Count:37
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 187 °CAverage value: 111 °C Grade Count:164
Deflection Temperature at 1.8 MPa (264 psi) 40.6 - 160 °CAverage value: 72.8 °C Grade Count:219
Vicat Softening Point 63.0 - 189 °CAverage value: 122 °C Grade Count:148
Heat Distortion Temperature 120 - 155 °CAverage value: 136 °C Grade Count:6
UL RTI, Electrical 65.0 - 125 °CAverage value: 112 °C Grade Count:13
UL RTI, Mechanical with Impact 65.0 - 120 °CAverage value: 112 °C Grade Count:8
UL RTI, Mechanical without Impact 65.0 - 120 °CAverage value: 111 °C Grade Count:11
Flammability, UL94 HB - 5VAAverage value: 5.50 Grade Count:343
Oxygen Index 17.0 - 34.0 %Average value: 25.9 % Grade Count:103
Glow Wire Test 550 - 960 °CAverage value: 887 °C Grade Count:150
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 240 °CAverage value: 211 °C Grade Count:25
Nozzle Temperature 199 - 240 °CAverage value: 210 °C Grade Count:30
Die Temperature 32.2 - 240 °CAverage value: 133 °C Grade Count:4
Melt Temperature 160 - 302 °CAverage value: 204 °C Grade Count:156
Mold Temperature 4.00 - 91.0 °CAverage value: 46.0 °C Grade Count:166
Drying Temperature 50.0 - 120 °CAverage value: 76.8 °C Grade Count:144
Moisture Content 0.0500 - 0.200 %Average value: 0.100 % Grade Count:15
Injection Pressure 2.76 - 150 MPaAverage value: 77.6 MPa Grade Count:84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-765A ABS - Flame Retardant
BASF Neopolen® P 92HD 105 Expanded Polypropylene (Europe)
Overview of materials for Polypropylene, Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Polypropylene with 40% Talc Filler

O4709 / 78375

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.