MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Wacker Powersil® 735 MEDIUM GRAY A/B Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® 735 MEDIUM GRAY A/B is a low viscous two-component compound with excellent processing properties. Its vulcanizates are noted for high tracking and erosion resistance, their good mechanical properties especially for high tear strength as well as for their excellent dielectric behavior.

Special features:

  • ready-to-use, two-component system
  • outstanding dielectrical properties
  • high tracking and erosion resistance
  • excellent mechanical properties, especially a high tear strength
  • excellent processing due to its low viscosity, also with suitable mixing and dosing equipment only

    Application:

    • cable accessories
    • insulators
    • outdoor and indoor use

    Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183-1 A
Viscosity  150000 cP
@Shear Rate 10.0 1/s
150000 cP
@Shear Rate 10.0 1/s
Component A; ISO 3219
 150000 cP
@Shear Rate 10.0 1/s
150000 cP
@Shear Rate 10.0 1/s
Component B; ISO 3219
 150000 cP
@Shear Rate 10.0 1/s
150000 cP
@Shear Rate 10.0 1/s
Mix; ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3939ISO 868
Tensile Strength at Break 8.00 MPa1160 psiISO 37
Elongation at Break 500 %500 %ISO 37
Tear Strength 30.0 kN/m171 pliASTM 624 B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+15 ohm-cm5.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.7
@Frequency 50 Hz
2.7
@Frequency 50 Hz
IEC 60250
Dielectric Strength 28.0 kV/mm711 kV/inIEC 60243
Dissipation Factor 0.00030
@Frequency 50 Hz
0.00030
@Frequency 50 Hz
IEC 60250
Arc Resistance >= 300 sec>= 300 secIEC 61621
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
post-cured 4hr at 200°C
Pot Life 4320 min4320 min
 
Descriptive Properties
Colorgray
Track Resistance1A 4.5IEC 60587

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage

PWACK9382 / 204911

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.