MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPC 1645 Polypropylene, Heterophasic Copolymer, Pipes
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Polypropylene PPC 1645 is a nucleated heterophasic (block) copolymer with a Melt Flow index of 0.3 g/10 min. This resin has a long-term heat stabilization package. It offers a very high stiffness while keeping good impact strength (even at very low temperatures) and excellent processability. Polypropylene PPC 1645 has been designed to allow pipe thickness reduction, resulting in cost savings.

Polypropylene PPC 1645 can also be used for blow molding and other extrusion applications.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccISO 1183
Oxidative Induction Time (OIT) >= 10 min
@Temperature 200 °C
EN 728
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 32.0 MPaISO 527-2
Elongation at Yield 8.0 %ISO 527-2
Tensile Modulus 1800 MPaISO 527-2
Flexural Modulus 1700 MPaISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature -20.0 °C
ISO 180
 >= 50.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -20.0 °C
ISO 179
 >= 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 3146

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes
Dow INSPIRE™ 112 Performance Polymer
Borealis BorECO™ BA212E Polypropylene Block Copolymer for Non-Pressure Pipes
Borealis Bormod™ HC904CF Polypropylene
Borealis RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems

PTOTAL845 / 130570

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.