MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Elexar® EL 1934F Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Elexar® EL-1934F is a high performance UL V-0 flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elexar EL-1934F is a high hardness, high density, high flow grade that is UV stabilized and RoHS compliant. This UL listed grade is easily colorable and is suitable for both molding and extrusion.

Features: Brominated; Electrically Insulating; Flame Retardant; Good Colorability; Good Flexibility; Halogenated; High Density; High Flow; High Specific Gravity; Medium Hardness; Sunlight Resistant (720 hours); UV Resistant

Uses: Cable Jacketing; Connectors; Insulation; Wire & Cable Applications

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70ASTM D2240
Tensile Strength at Break 9.65 MPaDie C, 20 in/min; ASTM D412
 8.11 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
 10.13 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
Elongation at Break 600 %Die C, 20 in/min; ASTM D412
 576 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
 588 %
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 970 V/milASTM D149
Dissipation Factor 0.0030
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 221 °FUL 1581
Brittleness Temperature <= -76.0 °FASTM D746
Flammability, UL94 V-0
Oxygen Index 3.0 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 420 °F
Middle Barrel Temperature 415 - 430 °F
Front Barrel Temperature 430 - 440 °F
Nozzle Temperature 430 - 445 °F
Zone 1 380 - 410 °F
Zone 2 390 - 420 °F
Zone 3 415 - 430 °F
Zone 4 420 - 430 °F
Zone 5 430 - 440 °F
Die Temperature 430 - 445 °F
Melt Temperature 430 - 445 °FProcessing Temp
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer
Saint-Gobain Tygon® PT-3350 Sanitary Silicone Tubing Formulation
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer

PTEKNO774 / 128955

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.