MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

E-Polymers TEKAMID® JN100 PPE+PA66 Filler Reinforced PA/PPE Alloy
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Polyphenylene Ether/PPO

Material Notes: Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.

JN-series: PA66/PPE, PA6/PPE alloy (Unreinforced, GF reinforced, MF reinforced)

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Water Absorption 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
Linear Mold Shrinkage 0.010 - 0.012 cm/cm0.010 - 0.012 in/in
Linear Mold Shrinkage, Transverse 0.0090 - 0.011 cm/cm0.0090 - 0.011 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 58.86 MPa8537 psiASTM D638
Elongation at Break 8.0 %8.0 %ASTM D638
Flexural Strength 110.85 MPa16077 psiASTM D790
Flexural Modulus 3.4335 GPa497.99 ksiASTM D790
Izod Impact, Notched 0.981 J/cm1.84 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 179 °C354 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 305 °C536 - 581 °F
Mold Temperature 75.0 - 120 °C167 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Ether, 30% Glass Filled
GEHR Plastics PPE-30GF Polyphenylene Ether, 30% Glass Fiber
E-Polymers TEKAMID® JN930 PPE+PA66 30% Glass Fiber Reinforced PA/PPE Alloy
Asahi Kasei Xyron™ L654V PPE/PS, High Stiffness, Low Warp, High Flow Chassis
Asahi Kasei Xyron™ L574Z PPE/PS, High Stiffness, Low Warp, High Flow Chassis

PEPOLZ011 / 103508

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.