MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Data provided by DuPont Packaging Polymers.

SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile strength, puncture strength, elongation and heat seal strength compared to conventional films. Ideal for lamination to other substrates such as Dartek® nylon film or Mylar® polyester film for vacuum packaging applications. SL, in converter combinations, is particularly suited for the vacuum packaging of processed meats.

Key Words: Linear Low Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/cc
Moisture Vapor Transmission 0.470 cc-mm/m²-24hr-atmASTM E96 Procedure E
Water Vapor Transmission 12.4 g/m²/dayASTM E96 Procedure E
Oxygen Transmission 236 cc-mm/m²-24hr-atmor 6200 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 38.1 microns
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 600 %ASTM D882
Tensile Modulus 0.170 GPaASTM D882
Dart Drop Test 100 g
Seal Strength >= 1800 g/25 mmSentinel Sealer Test
Film Tensile Strength at Break, MD 34.0 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 8.0 %ASTM D1003
Gloss 100 %20°; ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 38.1 µm Thickness
Dow Bynel® 41E710 Anhydride Modified LLDPE
Dow Appeel® 45D747 Polyolefin

PDU722 / 33156

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.