MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Matexcel MCP-006 Small Particle Size Nanoporous Carbon Powder
Categories: Other Engineering Material

Material Notes: Compared with traditional catalyst-supported activated carbon, the pore structure of small particle size nanoporous carbon powder is regular and orderly and the size is controllable, which can bring the following three advantages: 1. Compared with the diameter of the holes, the connecting holes between the holes and the holes are smaller, and the catalyst is confined in the holes after being loaded, which is not easy to agglomerate, and the life of the catalyst is significantly improved. 2. Compared with activated carbon, the new nanoporous carbon material has larger pores and can support more catalysts without being blocked by catalyst nanoparticles, and the pore size and connecting pore size can be adjusted according to the reactants and products. Precise size design of the required pore structure facilitates the entry and exit of reactants and products, and significantly improves the catalytic efficiency. 3. A large number of hydroxyl groups are modified on the inner wall of the pore, which is conducive to the uniform loading of the catalyst, and also provides a stronger bonding effect with the metal nanoparticles, so that the metal nanoparticles cannot move. Another advantage of using it as a drug catalyst is that there are very few precious metals remaining in the drug, and the treatment of precious metal residues in the later stage is relatively easy. Application scenarios: drug catalysts, hydrogen fuel cell catalysts.

Morphology: Powder

Key Words: Synonyms: Small Particle Size Nanoporous Carbon Powder
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK2023 / 300654

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.