Hostacom BJ 49 E NERO is a 30% chemically coupled, glass fiber reinforced PP copolymer, with excellent stiffness and good low temperature impact resistance. This grade is delivered in BLACK color version. Applications: Automotive Parts.Information provided by LyondellBasell. |