Pearlbond™ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbond™ D1160 is used for obtaining PU films by extrusion (blown and cast) for solvent-free adhesion, by heat-seal process. |