MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis FR4810 Low Smoke Zero Halogen Flame Retardant Jacketing Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: FR4810 is a thermoplastic, low smoke zero halogen (LSZH) flame retardant, black jacketing compound combining with flexibility and exceptional fluid resistance. The composition is based on the elements Carbon, Hydrogen, Oxygen, Silicon and Magnesium. Compounds based on these elements will therefore be the only significant constituents of the combustion fumes. Other elements may be present in concentrations less than 0.1%. Its excellent flame retardancy is achieved by an inorganic filler and a novel char-forming additive. Applications: 90°C rated jacket for energy cables with high flame retardancy required. The high operating temperatures and durability (abrasion resistance, hardness) of FR4810 makes it an attractive solution for energy cables installed in industrial areas, tunnels, ducts The ability of this compound to be used for both internal and external applications is valuable as it avoids the requirement of cable splicing at building service entrances. It can be used in areas sensitive to smoke or corrosive and toxic combustion products. In general, FR4810 has sufficient flame retardancy to satisfy bunched cable vertical burning tests. Specifications: FR4810 meets these applicable requirements when processed using sound extrusion practice and testing procedure: BS 6724, BS 7655, and LTS2VDE 0207 Teil 24 (HM4)

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccISO 1872-2/ISO 1183
Water Absorption 0.063 %
@Temperature 70.0 °C,
Time 1.21e+6 sec
ESCR 10% Igepal® >= 1.0 hour
@Temperature 50.0 °C
F20; IEC 60811-4-1/B
Melt Flow 0.10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 4815s; ISO 868
Tensile Strength at Break 2.20 MPaafter aging, 240h, 100°C; IEC 60811-1-2
 11.0 MPa50mm/min; IEC 60811-1-1
Elongation at Break 500 %IEC 60811-1-1
Flexural Modulus 200 MPaISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 500000 ohm-cmIEC 60093
Dielectric Strength >= 20.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °CISO 4589-3
Brittleness Temperature <= -35.0 °CASTM D746
Oxygen Index 35 %ASTM D2863
 
Descriptive Properties
Average Heat Release, kW/m2152ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
CO, kg/dm31.71ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
CO2, kg/dm30.011ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
Heat Combustion, MJ/dm327ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
High Temperature Pressure Test, %0.290°C;14 days;IEC 60811-3-1
Ignition Time, sec105ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
Max Heat Release, kW/m2213ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
Single Vertical Flame TestPassVW-1;0.76mm
Smoke Index15NES 711
Smoke Obscuration, m2/dmm3297ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
Toxicity Index2NES 713

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Casico™ FR4820 Natural Low Smoke Zero Halogen Flame Retardant Insulation Compound for Building Energy Cables
BASF Elastollan® 1154 D FHF TPUR Flame Retardant Halogen Free
BASF Elastollan® 1185 A FHF TPUR Flame Retardant Halogen Free
A. Schulman Diamond DIAMALOY 761 ABS/PC Alloy, Non-Halogen Flame Retardant with 5% PTFE
Fainplast Compounds HAX HF 20 Halogen Free PVC

PBOREA444 / 108703

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.