Initiator (80% active ingredient in water and di-tertbutyl peroxide) for (co)polymerization of acrylates and methacrylates. CAS number: 75-91-2 EINECS/ELINCS No: 200-915-7 Applications: Trigonox A-80 can be applied as an initiator in bulk and emulsion polymerization of styrene and styrene copolymers. Trigonox A-80 can also be used as an initiator for the polymerization of acrylates and methacrylates. Trigonox A-80 may also be used as an oxidizing agent for hydrocarbons and other chemical compounds or as a catalyst in the synthesis of lubricants Information provided by Nouryon |