MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Konson R-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80% Resorcinol, 20% SBR binder and dispersing agents

Use Characteristics: Konson® R-80 is a component of the bonding system resorcinol/ formaldehyde/ silica. In conjunction with a formaldehyde donor (e.g. Konson®HEXA-80 or Konson®HMMM-65) the resorcinol- formaldehyde- resin, responsible for the bonding of rubber to textile and steel cords, is formed during the curing process. This system is suitable for bonding all types of rubber to reinforcing materials, e.g. fabrics, glass fabrics and metals (e.g. steel-cords).

Processing Advantages: The predispersion of Resorcinol in a SBR binder allows quick absorption and excellent dispersion in the rubber. In this way, optimal activity of Resorcinol is assured.

Dosage levels: 3 - 4 phr

Applications: Tires, conveyor belts, V-belts, round belts, fire hoses, other reinforced hoses, flexible containers, fabric proofings.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Mooney Viscosity 50
@Temperature 50.0 °C
50
@Temperature 122 °F
Ash <= 0.30 %<= 0.30 %
Evaporation Loss <= 0.30 %<= 0.30 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 109 - 111 °C228 - 232 °F
Flash Point 127 °C261 °F
 
Descriptive Properties
Appearanceoff-white to red-brown granules
Content= 99%Resorcino
Sieve residue= 0.5 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS021 / 256066

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.