Elvacite® 2046 is a high molecular weight iso-butyl / n-butyl methacrylate copolymer. Elvacite® 2046 is useful in aluminum finishes, ceramic coatings, and aerosol snows. It is soluble in mineral spirits, VM & P Naphtha, and some alcohols.Information provided by Lucite International |