SABIC® LDPE 2201H0W is a grade without additives with a very good draw down ability. Films based on 2201H0W combine toughness with high tear strength and very good optical properties.
Application
SABIC® LDPE 2201H0W is typically used for thin packaging film purposes, where good optical properties are required.
SABIC® LDPE 2201H0W can typically be used for food applications due to very low migration levels.
Film properties
Film properties have been measured at film of 50 µm with a BUR of 3.
The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm.
This product is not intended for and must not be used in any pharmaceutical/medical applications.Information provided by SABIC |