MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Americhem Engineered Compounds ColorFast® NY1 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Injection molding nylon 6, with or without lube

All information provided by LTL Color Compounders, Inc. LTL was acquired by Americhem in 2014.

Key Words: Nylon
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccASTM D792
Water Absorption 1.7 %1.7 %@ 24 Hours; ASTM D570
Linear Mold Shrinkage 0.0015 - 0.0020 cm/cm0.0015 - 0.0020 in/in0.125 in.; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D785
Tensile Strength, Yield 79.3 MPa11500 psi2.0 in/min; ASTM D638
Elongation at Break 70 %70 %2.0 in/min; ASTM D638
Elongation at Yield 15 %15 %2.0 in/min; ASTM D638
Flexural Strength 118 MPa17100 psi2.0 in/min; ASTM D790
Flexural Modulus 2.78 GPa403 ksi2.0 in/min; ASTM D790
Izod Impact, Notched 0.534 J/cm
@Temperature 22.8 °C
1.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C155 °FUnannealed (0.250"); ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 293 °C500 - 560 °F
Middle Barrel Temperature 266 - 293 °C510 - 560 °F
Front Barrel Temperature 266 - 293 °C510 - 560 °F
Nozzle Temperature 260 - 288 °C500 - 550 °F
Melt Temperature 279 - 304 °C535 - 580 °F
Mold Temperature 37.8 - 93.3 °C100 - 200 °F
Drying Temperature 79.4 °C175 °F
Dry Time 2 - 4 hour2 - 4 hournominal; maximum drying time of 8 hours
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Shot Size 30 - 60 %30 - 60 %
Vent Depth 0.00381 - 0.00762 cm0.00150 - 0.00300 in
Screw Speed 60 - 120 rpm60 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLTLC023 / 104408

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.