MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® XE 4104 black 9992 PA610-GF40  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materials and its ecoprofile is very favorable when compared to similar products based on crude oil. The main features of Grilamid XE 4104 black 9992 are:
  • Low water absorption
  • Good heat, UV and chemical resistance
  • Easy processing
Grilamid XE 4104 black 9992 is particularly suitable for the manufacturing of technical injection molded parts in the application fields of:
  • Automotive
  • Electrical & Electronic goods
  • Mechanical engineering
  • Sports & leisure goods
  • Domestic appliances

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 155 MPaconditioned; ISO 2039-1
 215 MPadry; ISO 2039-1
Tensile Strength at Break 140 MPaconditioned; ISO 527-1/-2
 185 MPadry; ISO 527-1/-2
Elongation at Break 3.0 %dry; ISO 527-1/-2
 5.0 %conditioned; ISO 527-1/-2
Tensile Modulus 10000 MPaconditioned; ISO 527-1/-2
 12500 MPadry; ISO 527-1/-2
Charpy Impact Unnotched 80.0 kJ/m²dry; ISO 179/1eU
 85.0 kJ/m²conditioned; ISO 179/1eU
 85.0 kJ/m²
@Temperature -30.0 °C
conditioned; ISO 179/1eU
 90.0 kJ/m²
@Temperature -30.0 °C
dry; ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²dry; ISO 179/1eA
 16.0 kJ/m²conditioned; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
dry; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmdry; IEC 60093
 1.00e+12 ohm-cmconditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 5.00 kV/mmconditioned; IEC 60243-1
 36.0 kV/mmdry; IEC 60243-1
Comparative Tracking Index 600 Vconditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 130 °Clong term; EMS
 160 °Cshort term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 160 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Automotive electr. and electronics, lighting
 Compressed air systems
 Exterior
 Fuel systems
 Hydraulic systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Lighting
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesBio based Polyamide
Special CharacteristicsImproved heat resistance
 Improved UV resistance (outdoor use)
 Light stabilized or stable to light

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Pocan® BF 4232 000000 PBT, 30% Glass Fiber
EMS-Grivory Grilamid® L 16 LM PA12

PGRH124 / 156833

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.