- 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.
- The PA 616-GS can be processed on any laser sintering platform, but has been specifically engineered for EOS platforms.
- PA 616-GS is slightly less recyclable when compared to PA 615-GS, but produces a smooth part surface finish.
Information provided by Advanced Laser Materials (ALM). |