MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (Cond)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes:

Information provided by Ravago

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccDAM; ASTM D792
Water Absorption 1.0 %24 hrs, DAM; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm0.125 in, DAM; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ASTM D785
Tensile Strength at Break 12000 psiASTM D638
Elongation at Break 7.0 %ASTM D638
Flexural Strength 15000 psiASTM D790
Flexural Modulus 400000 psiASTM D790
Izod Impact, Notched 2.00 ft-lb/in73°F; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 462 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
BK
 HB
@Thickness 3.00 mm
BK
 HB
@Thickness 1.50 mm
NC
 HB
@Thickness 3.00 mm
NC
 
Processing PropertiesOriginal ValueComments
Melt Temperature 540 - 570 °F
Mold Temperature 150 - 210 °F
Drying Temperature 165 °F
Dry Time 2 - 4 hour
Moisture Content 0.20 %
Back Pressure 20.0 - 60.0 psi
Screw Speed 40 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 8018HS NC010 PA66-IGF14
Ascend Performance Materials Vydyne® R413H NT Impact Modified Nylon 66, Glass Filled
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (DAM)
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (DAM)
Ascend Performance Materials Vydyne® R413H BK07 Impact Modified Nylon 66, 13% Glass Filled

PENTA111 / 36148

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.