MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Hexcel® HexBond™ EA9685-1 Epoxy Fillet
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexBond™ EA 9685-1 Epoxy Fillet is a profile of semi-solid resin designed to be used in self-stiffened composite panels manufacturing. Its function is to fill the cavity between the panel and the stiffener. HexBond™ EA 9685-1 is a 180°C/ 356°F cure epoxy resin. When curing, due to its rheology, the resin fills the cavity without excess flow nor air trap.

Features:

  • Co-curable with most 180°C / 356°F cure prepreg systems
  • Allows saving work time
  • Assuring good reproducibility of structures
  • Spares the use of rolled resin film or UD tape

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  24.0 cP
@Temperature 125 °C
24.0 cP
@Temperature 257 °F
 40.0 cP
@Temperature 130 °C
40.0 cP
@Temperature 266 °F
 60.0 cP
@Temperature 101 °C
60.0 cP
@Temperature 214 °F
 60.0 cP
@Temperature 153 °C
60.0 cP
@Temperature 307 °F
 140 cP
@Temperature 158 °C
140 cP
@Temperature 316 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9266 / 322422

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.