MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBALLOY ECO PC (A20002) transparent 010000 100% PCR recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: KEBALLOY ECO PC (A20002) transparent is an unreinforced polycarbonate made of 100% PCR recyclate.

Properties: amorphous, impact resistant

Typical areas of application: Covers, Cover, Housing

Industries: Automotive, Electrical and electronics industry, Household appliances, Industry, Optics

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183-1
Linear Mold Shrinkage, Flow 0.00500 cm/cm0.00500 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.00400 cm/cm0.00400 in/inISO 294-4
Melt Flow 17.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
17.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 65.0 MPa9430 psiISO 527-1
Elongation at Break 75.0 %75.0 %ISO 527-1
Elongation at Yield 6.00 %6.00 %ISO 527-1
Modulus of Elasticity 2.40 GPa348 ksiISO 527-1
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 2.50 J/cm²11.9 ft-lb/in²ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 145 °C293 °FDIN EN ISO 11357-1
Flammability, UL94  HB
@Thickness 0.400 mm
HB
@Thickness 0.0157 in
IEC 60695-11-10
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90.0 %90.0 %Transparent, but not quatified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 320 °C536 - 608 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 120 °C248 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.0200 %<= 0.0200 %
Back Pressure <= 8.00 MPa<= 1160 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO661 / 326735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.