MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Delo® 400 SAE 10W-30
Categories: Fluid; Lubricant

Material Notes: Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.

They are formulated provide outstanding engine protection under both pre- and post-1998 EPA standards for exhaust particulate emissions for on highway diesel trucks, using both high and low sulfur diesel fuels.

Chevron Delo 400 SAE 10W, 20, 30, 40 and 50 are manufactured using carefully selected premium paraffinic base oils and an optimal blend of dispersant, detergent, oxidation inhibition, anti-wear, corrosion inhibition, and defoaming additives.

Chevron Delo 400 SAE 10W-30 is formulated with ISO-SYN™ base stocks.

Applications:

Chevron Delo 400 oils are mixed-fleet motor oils recommended for all four-stroke gasoline diesel engines operating under severe service and subjected to wide variations in climactic conditions.

Chevron Delo 400 oils are excellent for use in new advanced engines developed in response to 1998 lower exhaust particulate emissions with features such as four-valve heads, turbo charging, retarded fuel injections timing, direct injection, shorter piston crowns, higher power density, peak firing pressures up and beyond 2300 psi, intercooling, full electronic management of fuel systems, and exhaust particulate traps.

Chevron Delo 400 oils are also formulated for superior performance in older engines using both normal, high and low sulfur diesel fuels.

Chevron Delo 400 oils are not recommended for use in DDC two-stroke engines.

Chevron Delo 400 SAE 30 can be used in in powershift transmissions requiring Caterpillar TO 2 or an Allison C4 fluid.

Chevron Delo 400 SAE 10W, 20, 30, and 40 are authorized by USDA for use in federally inspected meat and poultry plants as H2 lubricants with no food contact.

Key Words: CPS Number: 235200; MSDS Number: 6711
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 30.6 °
Viscosity 3150 cP
@Temperature -20.0 °C
Cold Crank
Viscosity Measurement 150Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 70 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 11.1 cStASTM D445
Ash 1.34 %Sulfated Ash wt%
 
Chemical PropertiesOriginal ValueComments
Total Base Number 10.1ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -42.0 °CASTM D97
Flash Point 226 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.126 %
Zinc, Zn 0.14 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Addiplast Addilene H 560 Polypropylene Homopolymer
Addiplast Addilene H 462 M20 Polypropylene Homopolymer
ExxonMobil Exxtral™ HMU 301 Performance Polyolefin
Ensinger ENSIPRO® Polypropylene - Extruded Products (PP)

WCHEV009 / 74624

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.