System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Akro-Plastic Akromid® B3 GF 20 2 RM-D (3375) PA 6 Conditioned, 20% Glass Fiber Filled
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 20% Glass Fiber Filled
Material Notes:
AKROMID B3 GF 20 2 RM-D (3375) is a 20% glass fiber reinforced, UV-stabilized polyamide 6 with limited moisture absorption. Applications are interior and exterior parts in the automotive industry.
Information provided by Akro-Plastic GmbH
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.24
g/cc
ISO 1183
Filler Content
20 %
ISO 1172
Moisture Absorption
1.4 %
@Temperature 70.0 °C
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow
0.0030
cm/cm
ISO 294-4
Linear Mold Shrinkage, Transverse
0.0055
cm/cm
ISO 294-4
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
85.0
MPa
5 [mm/min]; ISO 527-1/2
Elongation at Break
3.5 %
5 [mm/min]; ISO 527-1/2
Tensile Modulus
1100
MPa
1 [mm/min]; ISO 527-1/2
Charpy Impact Unnotched
50.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
50.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched
10.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
12.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Thermal Properties
Original Value
Comments
Melting Point
220
°C
DIN EN 11357-1
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Daikin POLYFLON F-205 PTFE Fine Powder
Daikin POLYFLON F-201 PTFE Fine Powder
Chemours Teflon® PTFE 6C Resin for Lubricated Paste Extrusion
PAKRO158 / 182745
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.