MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotchkote™ KSIR88 Epoxy Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: 3M Scotchkote Epoxy Coating KSIR88 has been specifically developed as a high performance solvent based coating for pumps, valves fittings, tanks, and pipelines. Scotchkote epoxy coating KSIR88 combines good application characteristics with excellent corrosion protection and chemical resistance.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³
Solids Content 60 %60 %
Volatile Organic Compounds (VOC) Content 350 g/l350 g/las supplied
 393 g/l393 g/lthinned 10%
Thickness 125 microns4.92 mil
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourTouch Dry
 480 min8.00 hourHard Dry
 10100 min168 hourFull Cure
Shelf Life 24.0 Month
@Temperature 5.00 - 32.0 °C
24.0 Month
@Temperature 41.0 - 89.6 °F
 
Descriptive Properties
AppearanceOff White, Light Gray and Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35341 / 170088

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.