MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow Affinity™ PL 1280G Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: Affinity PL 1280G Polyolefin Plastomer is a Polyolefin Plastomer (POP) produced using INSITE Technology from Dow Plastics. It is specifically designed for use as a sealant layer in flexible structures for the packaging of meat and cheese, dry foods and consumer goods. Due to its excellent sealability at low temperatures, ultimate hot tack strength, optical properties and abuse resistance, it is particularly suitable for high speed form-fill-seal packaging machines. Applications: Cast Film. Complies with: Canadian HPFP No Objection; EU, No 10/2011; US FDA regulations for complete details.

Availability: Asia Pacific; Europe; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: EU No 102011; FDA FCN 424; HPFB (Canada) No Objection

Form: Pellets

Processing Method: Cast Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 5.80 MPa
@Thickness 0.0249 mm
841 psi
@Thickness 0.000980 in
ASTM D882
Film Tensile Strength at Yield, TD 5.30 MPa
@Thickness 0.0249 mm
769 psi
@Thickness 0.000980 in
ASTM D882
Film Elongation at Break, MD 470 %
@Thickness 0.0249 mm
470 %
@Thickness 0.000980 in
ASTM D882
Film Elongation at Break, TD 720 %
@Thickness 0.0249 mm
720 %
@Thickness 0.000980 in
ASTM D882
Elmendorf Tear Strength MD 78 g78 g0.00098; ASTM D1922
Elmendorf Tear Strength TD 410 g410 g0.00098; ASTM D1922
Dart Drop Test >= 290 g
@Thickness 0.0249 mm
>= 0.639 lb
@Thickness 0.000980 in
ISO 7765-1/B
Film Tensile Strength at Break, MD 48.0 MPa
@Thickness 0.0249 mm
6960 psi
@Thickness 0.000980 in
ASTM D882
Film Tensile Strength at Break, TD 30.0 MPa
@Thickness 0.0249 mm
4350 psi
@Thickness 0.000980 in
ASTM D882
Heat Seal Strength Initiation Temperature 87.8 °C190 °FASTM D1525
 
Thermal PropertiesMetricEnglishComments
Melting Point 96.1 °C205 °F
Vicat Softening Point 81.1 °C178 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %4.0 %Cast Film
Gloss 91 %
@Thickness 0.0249 mm
91 %
@Thickness 0.000980 in
20°, Cast Film; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF380 / 311073

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.