MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C/8 hr.
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: High-Strength, Cold Formable Strip Alloy

Industry Specifications: USA Aerospace: AMS 4914A.

Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vessels and other fabricated sheet metal structures up to 300°C.

Mechanical property data reported Typical heat treatment for this alloy: Solution Treatment: 790°C for 3-20 min, air cool. Age Treatment: 480-620°C for 4-16 hrs.

Data provided by TIMET.

Key Words: 15-3-3-3
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.78 g/ccTypical
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 1000 MPaspecified minimum
 1160 MPaTypical
 145 ksi
@Temperature 316 °C
 155 ksi
@Temperature 204 °C
 170 ksi
@Temperature 93.3 °C
 185 ksi
@Temperature -17.8 °C
 210 ksi
@Temperature -73.3 °C
 275 ksi
@Temperature -184 °C
Tensile Strength, Yield >= 965 MPa
@Strain 0.2 %
specified minimum
 1050 MPa
@Strain 0.2 %
Typical
 125 ksi
@Strain 0.2 %,
Temperature 316 °C
 140 ksi
@Strain 0.2 %,
Temperature 204 °C
 148 ksi
@Strain 0.2 %,
Temperature 93.3 °C
 170 ksi
@Strain 0.2 %,
Temperature -17.8 °C
 175 ksi
@Strain 0.2 %,
Temperature -73.3 °C
 200 ksi
@Strain 0.2 %,
Temperature -184 °C
Elongation at Break >= 7.0 %specified minimum
 11 %Typical
 5.0 %
@Temperature -184 °C
 7.6 %
@Temperature 316 °C
 8.0 %
@Temperature -73.3 °C
 9.5 %
@Temperature 204 °C
 11 %
@Temperature -17.8 °C
 11 %
@Temperature 93.3 °C
Modulus of Elasticity 107 GPa
Fatigue Strength 755 MPaLimit; test specifics not reported
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.70 µin/in-°F
@Temperature 22.8 - 93.3 °C
 5.20 µin/in-°F
@Temperature 22.8 - 316 °C
 5.50 µin/in-°F
@Temperature 22.8 - 538 °C
 6.10 µin/in-°F
@Temperature 22.8 - 760 °C
 8.60 µm/m-°C
@Temperature 20.0 °C
 9.20 µm/m-°C
@Temperature 20.0 - 250 °C
 9.90 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.500 J/g-°C
 0.120 BTU/lb-°F
@Temperature 22.8 °C
 0.130 BTU/lb-°F
@Temperature 204 °C
 0.160 BTU/lb-°F
@Temperature 538 °C
 0.190 BTU/lb-°F
@Temperature 760 °C
Thermal Conductivity 8.30 W/m-K
 60.0 BTU-in/hr-ft²-°F
@Temperature 22.8 °C
 74.0 BTU-in/hr-ft²-°F
@Temperature 204 °C
 110 BTU-in/hr-ft²-°F
@Temperature 538 °C
 138 BTU-in/hr-ft²-°F
@Temperature 760 °C
Maximum Service Temperature, Air 288 °C
Beta Transus 760 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 2.5 - 3.5 %
Carbon, C <= 0.050 %
Chromium, Cr 2.5 - 3.5 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.25 %
Nitrogen, N <= 0.050 %
Other, each <= 0.10 %
Other, total <= 0.40 %
Oxygen, O <= 0.13 %
Tin, Sn 2.5 - 3.5 %
Titanium, Ti 72.6 - 78.5 %Calculated as remainder
Vanadium, V 14 - 16 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 482°C/16 hr
TIMET TIMETAL® 1100 Titanium Alloy (Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si), Beta Anneal + 1400°F
TIMET TIMETAL® 17 Titanium Alloy (Ti-5Al-2Sn-4Mo-2Zr-6Mo); STA
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 496°C/8 hr
TIMET TIMETAL® 829 (Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si) Titanium Alloy

NTIME153B / 19286

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.