MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik Polymer ST 77
Categories: Polymer

Material Notes: Applications: Polymer ST 77 is free of phthalates and is highly recommended for demanding applications where a balanced stress-strain behavior is required as in transport and assembly applications. Examples for the use of Polymer ST 77-based formulations are the assembly of superstructural parts, bumpers, etc. Mechanical fastening is often avoided as it could cause damage to the materials used. In addition, it could negatively affect the design.

Benefits: For assembly applications, adhesives must be processed quickly and provide rapid strength development. In these cases, Polymer ST 77 is a suitable solution as its stress-strain behavior can be tuned to the application needs.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 40000 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3.20 MPa
Elongation at Break 475 %
 
Descriptive Properties
Appearancecolorless, transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIM108 / 197312

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.