MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Celanese Coolpoly® D4302 Thermally Conductive Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows design freedom in applications previously restricted to metals. The D series is electrically non-conductive and can be used for its dielectric properties.

CoolPoly D4302 is a thermally conductive injection molding resin based on a PBT matrix. CoolPoly D4302 is electrically insulative. Thermally conductive polymers like CoolPoly D4302 cool faster than standard injection molding grade resins.

Information provided by Cool Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ISO 1183
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm0.0070 - 0.010 in/inASTM D551
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 42.0 MPa6090 psiISO 527-1
Elongation at Break 1.45 %1.45 %ISO 527-1
Tensile Modulus 6.00 GPa870 ksiISO 527-1
Flexural Strength 61.0 MPa8850 psiISO 178
Flexural Modulus 3.40 GPa493 ksiISO 178
Charpy Impact Unnotched 2.40 J/cm²11.4 ft-lb/in²ISO 179-1
Charpy Impact, Notched 0.280 J/cm²1.33 ft-lb/in²ISO 179-1
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.31 J/g-°C0.313 BTU/lb-°FASTM E1461
Thermal Conductivity 2.60 W/m-K18.0 BTU-in/hr-ft²-°FASTM E1461
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 200 - 210 °C392 - 410 °F
Middle Barrel Temperature 204 - 227 °C399 - 441 °F
Front Barrel Temperature 216 - 238 °C421 - 460 °F
Melt Temperature 216 - 238 °C421 - 460 °F
Mold Temperature 27.0 - 66.0 °C80.6 - 151 °F
Drying Temperature 82.0 °C180 °F
Dry Time 4 hour4 hour
Dew Point -18.0 °C-0.400 °F
Injection Pressure 35.0 - 82.0 MPa5080 - 11900 psi
Hold Pressure 14.0 - 28.0 MPa2030 - 4060 psi
Back Pressure 0.000 - 0.350 MPa0.000 - 50.8 psi
Screw Speed 40 - 100 rpm40 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Coolpoly® D1202 Thermally Conductive Polypropylene
Celanese CoolPoly® E1201 Thermally Conductive Polypropylene
Celanese CoolPoly® E3603 Thermally Conductive Polyphthalamide (PPA)
Celanese CoolPoly® E4301 Thermally Conductive Polybutylene Terephthalate
Celanese CoolPoly® E4501 Thermally Conductive Polycarbonate

PCOOL08 / 29008

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.