MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Magnesium EA65RS-T4, Extruded
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes:

Key Words: Aerospace Alloy; Mg
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.92 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 515 MPa
Tensile Strength, Yield 460 MPa
@Strain 0.2 %
Elongation at Break 5.0 %in 50 mm
Tensile Modulus 45.0 GPaTypical Mg alloy
Poissons Ratio 0.32Calculated
Shear Modulus 17.0 GPaEstimated from similar Mg alloys.
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.00 J/g-°CTypical Mg alloy value.
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.0 %
Magnesium, Mg 84 %As Remainder
Yttrium, Y 5.9 %
Zinc, Zn 5.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium EA55RS-T4, Extruded
Magnesium Elektron Elektron® ZK60A Magnesium Alloy, UNS M16600
Overview of materials for Magnesium Alloy
SAE SiC/AZ91 Magnesium Matrix Composite, as cast
Magnesium AZ31B-F, Extruded Solid Shapes

MMEA53 / 12375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.