MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE EE-1290 BLK 111 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink EE-1290 BLK 111 is a general purpose thermoplastic elastomer designed for automotive applications, including exterior extruded components. Sarlink EE-1290 BLK 111 is a high hardness, high density grade with good UV resistance and can also be injection molded.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Processability; High Density; High Specific Gravity; High Hardness; UV Stabilized

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping

RoHS Compliance: RoHS Compliant

Automotive Specifications: ASTM D4000 Color: Black

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccASTM D792
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 1800 psiASTM D412
Tensile Stress at Strain 660 psi
@Strain 100 %
ASTM D412
Elongation at Break 550 %ASTM D412
Tear Strength 270 pliDie C; ASTM D1004
 
Processing PropertiesOriginal ValueComments
Processing Temperature 420 - 440 °FMelt, Injection
Rear Barrel Temperature 390 - 410 °FInjection
Middle Barrel Temperature 400 - 420 °FInjection
Front Barrel Temperature 410 - 430 °FInjection
Nozzle Temperature 420 - 440 °FInjection
Zone 1 380 - 400 °FExtrusion
Zone 2 390 - 410 °FExtrusion
Zone 3 400 - 420 °FExtrusion
Zone 4 400 - 420 °FExtrusion
Zone 5 410 - 430 °FExtrusion
Die Temperature 420 - 440 °FExtrusion
Mold Temperature 95.0 - 150 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 125 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 120 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1023 / 237514

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.