MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 4699 X 80222 Syndiotactic Polystyrene (SPS), Reinforced - Platable
Categories: Polymer; Thermoplastic; Polystyrene (PS); Syndiotactic Polystyrene (SPS)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D 792
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 12000 psiASTM D 638
Elongation at Break 2.0 %ASTM D 638
Tensile Modulus 1250 ksiASTM D 638
Flexural Strength 19500 psiASTM D 790
Flexural Modulus 1250 ksiASTM D 790
Izod Impact, Notched 1.75 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 7.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 11.0 µin/in-°FE 831
CTE, linear, Transverse to Flow 46.0 µin/in-°FE 831
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 560 - 620 °F
Mold Temperature 160 - 300 °F
Drying Temperature 180 °F
@Time 7200 sec
Moisture Content 0.020 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled
I. Stern GPPS-004 General Purpose Crystal Polystyrene
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance
Overview of materials for Acetal Copolymer, PTFE Filled

PQZWA10011 / 90451

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.