MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECACOMP PE ID blue 1049852 Polyethylene, Mineral Filled
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes:
  • detectable via metal detector
  • x-ray detectable
  • Explanation of food contact according to FDA and EU 10/2011 on request
  • good toughness
  • low water absorption
  • good chemical resistance
Target Industries:
  • food technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³
Linear Mold Shrinkage, Flow 0.035 cm/cm0.035 in/inDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inDIN EN ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 19.0 MPa2760 psiDIN EN ISO 527-1
Elongation at Break 7.8 %7.8 %DIN EN ISO 527-1
Modulus of Elasticity 1.20 GPa174 ksiDIN EN ISO 527-1
Charpy Impact Unnotched 2.40 J/cm²11.4 ft-lb/in²DIN EN ISO 179-1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 135 °C275 °F
Maximum Service Temperature, Air 80.0 °C176 °Flong term
 100 °C212 °Fshort term
Glass Transition Temp, Tg -70.0 °C-94.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 240 °C356 - 464 °F
Mold Temperature 20.0 - 60.0 °C68.0 - 140 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
 
Descriptive Properties
Colorblue
Detectability3.1 mm Al4 x 4 x 4 mm, x-ray detectable
 4.5 mm Al4 x 4 x 4 mm, metal detectable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9042 / 318970

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.