MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Struktol STRUKSILON 8120 Silicone Stabilizer for PU Foam
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: STRUKSILON 8120 was developed as universal silicone stabilizer of high potency for the production of conventional as well as flame retardant flexible polyurethane slabstock foam based on polyether polyols.

Applications: STRUKSILON 8120 is applicable in systems for nearly all known flexible PU slabstock foam applications and technologies like production of seats, chairs, mattresses etc. in the furniture and automotive industry and for all kinds of damping devices.

Information provided by Struktol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.023 g/cc
Viscosity 900 cP
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 100 °CDIN/ISO 2562
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.449
@Temperature 25.0 °C
 
Descriptive Properties
AppearanceClear, colorless to slightly yellow liquid
Turbidity Point °C34

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Struktol STRUKSILON 8026 Silicone Stabilizer for PU Foam
Struktol STRUKSILON 8104 Silicone Stabilizer for PU Foam
Struktol STRUKSILON 8002 Silicone Stabilizer for PU-Rigid Foam
Struktol STRUKSILON 8118 Silicone Stabilizer for PU Foam
Overview of materials for PVC, Foam Grade

PSTRUK81 / 69308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.