PPS-SG401R87 PPS is a 40% advanced glass fiber reinforced linear polyphenylene sulfide and elastomer, both with PPS high rigidity, high heat resistance, corrosion resistance and other excellent properties and has a good impact resistanceInformation provided by Shandong Sciengy New Materials Co. Ltd |