MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum ALFA-I™ Stainless Steel Type 406
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization.

Applications:automotive exhaust system components, furnace parts, heat exchangers, recuperator parts, kiln lining, refractory reinforcement fibers.

Information provided by Allegheny Ludlum

Key Words: UNS K91470
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.48 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 88
Tensile Strength, Ultimate 519 MPaLongitudinal, Unwelded
 524 MPa
 538 MPaTransverse, Welded
 551 MPaLongitudinal, Welded
Tensile Strength, Yield 368 MPaLongitudinal, Unwelded
 379 MPa
 402 MPaTransverse, Welded
 409 MPaLongitudinal, Welded
Elongation at Break 28 %in 2"
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000111 ohm-cm
@Temperature 20.0 °C
 0.000112 ohm-cm
@Temperature 204 °C
 0.000118 ohm-cm
@Temperature 427 °C
 0.000129 ohm-cm
@Temperature 649 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 20.0 - 200 °C
 12.8 µm/m-°C
@Temperature 20.0 - 500 °C
 14.4 µm/m-°C
@Temperature 20.0 - 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 3.0 %
Carbon, C 0.025 %
Chromium, Cr 13 %
Iron, Fe 83.24 %As Remainder
Manganese, Mn 0.035 %
Silicon, Si 0.30 %
Titanium, Ti 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
406 Stainless Steel
AK Steel 13-4 SR® Ferritic Stainless Steel
ATI Allegheny Ludlum ALFA-II™ Stainless Steel Type 406
ATI Allegheny Ludlum Stainless Steel Ohmaloy® 40 Resistance Alloy
ATI Allegheny Ludlum Ohmaloy® 30 Resistance Alloy

NL1038 / 17806

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.