Hostacom CR 1171 G1 D71499 is a 15% talc filled PP copolymer medium melt flow, high impact/stiffness balance, improved UV resistance. Product is available as a customized color matched, pellet form. This grade is delivered in D71499 color version.Information provided by LyondellBasell. |