MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil SpectraSyn Plus™ 4 Advanced Polyalphaolefin (PAO) Fluid
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices translate into improved flow at low temperatures and increased film thickness at high temperatures. SpectraSyn Plus™ Advanced PAO provide superior lubrication as the primary basestocks for synthetic lubricants used in passenger car engines, heavy-duty diesel engines, transmissions, and a variety of industrial applications. SpectraSyn Plus™ Advanced PAO can be use for upgrading mineral oil or Group III basestock for improved low temperature and volatility performance.

Appearance: Bright & Clear

Availability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.820 g/cc
@Temperature 15.6 °C
ASTM D4052
Viscosity 1.24 cPHigh-Temp. High Shear; ASTM D5481
 2023 cP
@Temperature -40.0 °C
Apparent Viscosity by Mini-Rotary Viscometer; ASTM D4684
Brookfield Viscosity 2538 cP
@Temperature -40.0 °C
ASTM D2983
Viscosity Measurement 126Index; ASTM D2270
Kinematic Viscosity 2430 cSt
@Temperature -40.0 °C
ASTM D445
Kinematic Viscosity at 40°C (104°F) 17.2 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 3.9 cStASTM D445
Vapor Pressure 0.200 torr
@Temperature 150 °C
ASTM D2879
Evaporation Loss 15.2 %
@Temperature 205 °C,
Time 23400 sec
ASTM D972
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.050[mg KOH/g]; ASTM D974 (mod)
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.1ASTM D924
Dielectric Breakdown 41200 V
 
Thermal PropertiesOriginal ValueComments
Pour Point <= -76.0 °FASTM D5950/D97
Flash Point 442 °FCOC; ASTM D92
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.453ASTM D1218
 
Descriptive Properties
Aniline Point248°FASTM D611
Cold Cranking Simulator1290 cP-31°F, ASTM D5293
 733 cP-13°F, ASTM D5293
 804 cP-22°F, ASTM D5293
Color<0.5ASTM D1500
CompositionWater<50 ppm, ASTM D6304 (mod)
Density Correction Factor0.000644 (g/cc)/°CASTM D1250
Fire Point489°FCOC, ASTM D92
Kauri-Butanol Value13ASTM D1133
Noack Volatility<12%ASTM D5800/DIN 51581

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow UCON™ LB-65 Fluids and Lubricants
ChevronTexaco 5606G Aircraft Hydraulic Oil
Anderol ANDEROL® FGH 22 Synthetic Food Grade Hydraulic Fluid, ISO 22
ExxonMobil SpectraSyn™ 8 Polyalphaolefin (PAO) Fluid
ExxonMobil SpectraSyn™ 4 Polyalphaolefin (PAO) Fluid

PEX99685 / 175921

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.