MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Superior Flux Superior HASL No. 1 Hot Air Solder Leveling Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • A Non-Chloride, VOC-Free Hot Air Flux.
  • A water-soluble HASL that requires no organic solvents for cleaning.
  • Completely non-ionic formulation.
  • Non-hazardous and safe to handle.
Description: Superior HASL No.1 Flux is a Non-Chloride activated water-soluble, non-flammable, heat-stable organic flux specially formulated for Hot-Air Solder Level soldering processes in vertical and linear PC Fabrication processes. Formulated for high temperature solders, this flux is stable and active during the heat-cycle to promote solder wetting to metal surfaces rapidly and actually assists the solder process by relieving surface tension of the solder.

Applications: When soldering, preheating the applied flux prior to immersion in the solder reduces or eliminates spattering from the process. Superior HASL No. 1 is completely water-soluble and is easily removed from post-solder surfaces using DI water. A water temperature of 60ºC/140ºF is recommended for optimum results and cleanliness. Post solder finish is bright, shiny and smooth.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.085 - 1.105 g/cc
pH 0.80 - 1.8
 
Descriptive Properties
FormClear Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSFLUX118 / 185802

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.