Notes: Medalist MD-84300 series are high performance thermoplastic elastomer designed specifically for extrusion and injection molded electrical applications in the medcial and healthcare industry. The Medalist MD-84300 series are a better alternative to traditional TPVs used in such applications. Medalist MD-84348 is a low hardness, low density grade with good electrical properties and can be sterilized by autoclave, ETO, or gamma radiation. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Autoclave Sterilizable; Chemical Resistant; Electrically Insulating; Ethylene Oxide Sterilizable; Good Color Stability; Good Colorability; Good Sterilizability; Halogen Free; High Tensile Strength; Low Density; Low Flow; Low Hardness; Low Specific Gravity; Radiation (Gamma) Resistant; Slip Uses: Flexible Jacketing; Medical/Healthcare Applications; Pharmaceuticals; Wire & Cable Applications Agency Ratings: ISO 13485 RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion; Injection Molding Preliminary data. Information provided by Teknor Apex |