MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Supol HR580 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Product Description: SUPOL HR580 is a high flow, mineral filled, polypropylene compound for injection molding. This grade is designed for painted bumper fascia applications.

Availability: North America

Filler/Reinforcement: Mineral

Features: High Flow; High Impact Resistance; Medium Rigidity; Paintable

Uses: Automotive Bumper

Processing Method: Injection Molding

Information provided by LyondellBasell Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Melt Flow 42 g/10 min
@Load 2.16 kg,
Temperature 230 °C
42 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.0 MPa2760 psiISO 527-2
Elongation at Break 100 %100 %ISO 8986-2
Flexural Modulus 1.80 GPa261 ksiISO 178
Izod Impact, Notched (ISO)  6.51 kJ/m²
@Temperature -30.0 °C
3.10 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 35.7 kJ/m²
@Temperature 22.8 °C
17.0 ft-lb/in²
@Temperature 73.0 °F
ISO 180

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLYON800 / 311493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.